Fly ash is the finely divided
residue that results from the combustion of ground or powdered coal and is transported from the boiler by fle gases. For these specifications, it is divided into two types, Type A and Type B, the type to be designated for specific usage.
Type A: This type of fly ash is used as an admixture in Portland cement concrete to promote workability and plasticity. The material shall meet the requirements of ASTM: C 618.
Type B: This type of fly ash is used as a partial replacement for Portland cement in Portland cement concrete. The material shall meet the following requirements:
A. Chemical.
Silicon dioxide (SiO2) + Aluminum oxide (Al2O3) + Iron oxide (Fe2O3) minimum, percent
70.00 Silicon dioxide (SiO2) minimum, percent Aluminum oxide (Al2O3) minimum, percent Magnesium oxide (MgO) maximum, percent 3.00 Sulphur trioxide (SO3) maximum, percent 3.00 Loss on ignition, maximum, percent 6.00 Moisture content, maximum, percent 3.00 Available alkalies as Na2O, maximum, percent 1.50
B. Physical.
Percent retained on No. 325 sieve, 45uM maximum, percent 20.00 Pozzolanic activity index strength of lime-pozzolan at 7 days, minimum, psi 800.00 Change of drying shrinkage of mortar bars at 28 days, maximum, percent +0.03
Soundness Autoclave expansion of mortar bars maximum, percent 0.50
C. Tests. Laboratory tests for acceptance and project control will be selected by the
engineer. Methods of tests shall be in accordance with the following:
Sampling and testing fly ash
ASTM: C 311